Hastelloy Price | Origin | Price in INR (per kg) |
Price in USD (per kg) |
Price in Euro (per kg) |
---|---|---|---|---|
Hastelloy Alloy Price in India | Indian | Rs 4000/- | $58 | €50 |
Hastelloy Price in Japan | Japanese | Rs 5500/- | $81 | €69 |
Hastelloy Price in UK / Europe | European | Rs 6000/- | $88 | €75 |
Hastelloy Price in USA | USA | Rs 7000/- | $103 | €89 |
Alloy* | C% | Co% | Cr% | Mo% | V% | W% | Ai% | Cu% | Nb % | Ti% | Fe% | Ni% | Other% |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|
B | 0.1 | 1.25 | 0.6 | 28 | 0.3 | - | - | - | - | - | 5.5 | rest/bal | Mn 0.80; Si 0.70 |
B2 / B-2 | 0.02 | 1 | 1 | 26.0-30.0 | - | - | - | - | - | - | 2 | rest/bal | Mn 1.0, Si 0.10 |
C | 0.07 | 1.25 | 16 | 17 | 0.3 | 40 | - | - | - | - | 5.75 | rest/bal | Mn 1.0; Si 0.70 |
C4 / C-4 | 0.015 | 2 | 14.0-18.0 | 14.0-17.0 | - | - | - | - | - | 0..70 | 3 | rest/bal | Mn 1.0 ; Si 0.08 |
C276 / C-276 | 0.02 | 2.5 | 14.0-16.5 | 15.0-17.0 | 0.35 | 3.0-4.5 | - | - | - | - | 4.0-7.0 | rest/bal | Mn 1.0; Si 0.05 |
F | 0.02 | 1.25 | 22 | 6.5 | - | 0.5 | - | - | 2.1 | - | 21 | rest/bal | Mn 1.50; Si 0.50 |
G | 0.05 | 2.5 | 21.0-23.5 | 5.5-7.5 | - | 1 | - | 1.5-2.5 | 1.7-2.5 | - | 18.0-21.0 | rest/bal | Mn 1.0-2.0; P0.04; Si 1.0; |
G2 / G-2 | 0.03 | - | 23.0-26.0 | 5.0-7.0 | - | - | - | 0.70-1.20 | - | 0.70-1.50 | rest/bal | 47.0-52.0 | Mn 1.0; Si 1.0 |
N | 0.06 | 0.25 | 7 | 16.5 | - | 0.2 | - | 0.1 | - | - | 3 | rest/bal | Mn 0.40; Si 0.25; B 0.01 |
S | 0.02 | 2 | 15.5 | 14.5 | 0.6 | 1 | 0.2 | - | - | - | 3 | rest/bal | Mn 0.50; Si 0.40; B0.0009; La 0.02 |
W | 0.06 | 1.25 | 5 | 24.5 | - | - | - | - | - | - | 5.5 | rest/bal | Mn 0.050; Si 0.50 |
X | 0.1 | 1.5 | 22 | 9 | - | 0.6 | - | - | - | 18.5 | - | rest/bal | Mn 0.6; Si 0.60 |
B-3 | B-3 is a member of the nickel-molybdenum family of Hastelloy alloys. Hastelloy B-3 is the alloy in the Hastelloy family that shows best resistance to hydrochloric acid. |
---|---|
Alloy C-276 | Alloy C-276 is a nickel-molybdenum-chromium wrought alloy that is generally used as corrosion-resistance. Alloy c-276(Hastelloy C276) is among the more well known Hastelloy grades for general corrosion service. Hastelloy C-276 alloy is an improved wrought version of Hastelloy alloy C. |
Alloy C-4 | Alloy C-4 is a nickel-chromium-molybdenum Hastelloy alloy with good high-temperature stability. The Alloy C-4 is an Hastelloy grade, that resists the formation of grain-boundary precipitates in weld heat-affected zones. Alloy C-4 also has excellent resistance to stress-corrosion cracking and to oxidizing atmospheres. Alloy C-4 is also used in a varity of chemical process environments. |
Alloy G | Alloy G is an nickel-chromium-iron-molybdenum alloy developed for corrosion resistance in both oxidizing and reduceing media. Alloy G shows good resistance to sulfuric and phosphoric acid. Alloy G may further handle both acid and alkaline solutions. |
Alloy X | Alloy X - a nickel-chromium-iron-molybdenum alloy - has been developed to combine oxidation resistance, fabricability and high-temperature strength. Alloy X is also It has also been found to be resistant in petrochemical applications. |
Hastelloy C | 1320 - 1350 | 2410 - 2460 |
© Copyright @ Neelcon Steel All Rights Reserved. | Design & SEO by Mesotek